Low-temperature TPU used for heel counter stiffeners (gangbao港宝)

Low-temperature TPU used for heel counter stiffeners (gangbao港宝) has its core value in lowering the heat activation temperature to the 70–110°C range, with some ultra-low-temperature grades reaching a crystalline melting point range of 50–60°C. This protects heat-sensitive shoe uppers while providing the rigidity and resilient rebound needed for heel counter shaping.

Key Physical Properties

The main indicators can be referenced against Group Standard T/NHXY 4-2021 (Polymer Low-Temperature TPU Hot-Melt Adhesive Heel Counter Stiffener):

Item Typical Indicator / Range
Bonding activation temperature 70–90°C; some film products have a nominal melting temperature of 80–110°C
Shore A hardness 94–98 HA
Tensile strength Longitudinal ≥480 MPa; transverse ≥320 MPa
Flex resistance Low temperature (0±1)°C ≥15,000 cycles; room temperature (23±2)°C ≥40,000 cycles
Bond strength (N/25 mm) Genuine leather ≥60; PU synthetic leather ≥50; cotton fabric ≥50
Bursting force 0.2–0.4 mm ≥100 N; >0.4–1.0 mm ≥120 N; >1.0 mm ≥160 N

Core Advantages

① Protection of heat-sensitive uppers
Conventional heel counter stiffeners require relatively high hot-pressing temperatures, which can easily cause scorching, shrinkage, or discoloration of flyknit, engineered mesh, ultra-thin PU, microfiber, and similar uppers. Low-temperature TPU keeps the hot-pressing temperature within the upper’s tolerance window, reducing defect rates while also lowering the energy consumed in mold heating and cooling and shortening the hot-pressing cycle.

② Balanced shaping rigidity and flexural rebound
High hardness (94–98 HA) provides the supporting framework for the heel counter, while the TPU matrix itself has elastic recovery capability. This helps the bonded shoe component resist hardening, whitening, or delamination at seams after repeated flexing. The standard’s requirements of 40,000 cycles at room temperature and 15,000 cycles at low temperature are quantitative constraints on this balance.

③ Low-temperature performance
TPU generally offers better low-temperature flexibility than PVC. Low-temperature TPU for heel counters typically remains free from embrittlement and cracking at around -40°C to -50°C, and some formulations retain elasticity at even lower temperatures. This makes it suitable for shoes worn in cold regions, outdoor footwear, and scenarios involving low-temperature storage and transportation.

④ Environmental and processing friendliness
It is generally solvent-free and bonds through phase-change softening during hot pressing, with no release of harmful volatile substances. The adhesive film or sheet also tends to have good thickness uniformity and resists tensile deformation during die-cutting, making it compatible with automated cutting and continuous hot-pressing lines.

Selection and Incoming Material Control Points

The performance of low-temperature TPU heel counter stiffeners depends heavily on TPU content and formulation purity. Sheets containing recycled material or excessive filler may look similar, but their softening rate in hot water will be slower; if hot-press activation is insufficient, shaping performance and durability will decline. A simple incoming-material check is to cut samples of the same thickness into small pieces and immerse them in freshly boiled water to observe the softening rate—faster softening generally indicates higher effective TPU content and purer formulation.

Thickness selection should match the shoe type: 0.4–0.8 mm is mostly used for lightweight footwear, women’s shoes, and children’s shoes; 1.0–1.5 mm is intended for boots, hiking shoes, or shoe styles requiring stronger heel support.


In summary, low-temperature TPU for heel counters is a shaping material characterized by a 70–90°C-class activation temperature as the processing entry point, a 94–98 HA high hardness plus flex resistance and rebound as the mechanical balance point, and low-temperature resistance down to below -40°C as the environmental adaptability. During selection, it is advisable to first confirm the upper’s maximum temperature tolerance, then compare bonding strength and flex resistance against the group standard, and assess TPU purity control capability.


Post time: Nov-28-2026